Revisions log for Answer #1826

This is the answer to the question Why are there micro cracks on the facade being insulated with EPS?

Revision 1

2022‑08‑27 12:58
KevinXX
Active REV1
Initial text

For insulation system, mesh with a tensile load (on the base and weft 2000N) is 165gr.

The quality depends on the manufacturer. It is likely that the top layer began to "dry out" / give up water very quickly. And the deeper layers were still wet, with the release of moisture and ripped.

Please clarify the order of your actions:

— applied a layer of glue (how thick?)

— Drowned the mesh (did it remain visible?)

— and then reapplied glue after the tear?

How thick was the overall layer of glue?